1. Magnesite
The magnesium content of the raw magnesite ore mined by our factory reaches more than 46%. Advanced crushing equipment is used to crush the raw ore into a uniform size block and enter the reflection cellar, which reduces the over-burning rate and under-burning rate of the product and ensures that the The processed magnesium oxide content of the finished product is above 85%. The magnesite is manually screened to separate the ore containing other impurities. Haicheng magnesium oxide enhances the safety and stability of the product.
2. Fuel
Select high-quality coal and sign long-term purchase and sales contracts with state-owned coal manufacturers, which not only ensures the quality of the fuel, but also stabilizes the price of the fuel.
Magnesium oxide physical and chemical indicators
Specifications | MgO≥ | activeMgO≥ | f-CaO≤ | loss on ignition≤ | particle size | color |
QM-92 | 92 | 68 | 1.00 | 1—2 | 200 mesh pass rate 90-95% | yellowish |
QM-90 | 90 | 68 | 1.00 | 2.50—4 | 200 mesh pass rate 90-95% | yellowish |
QM-85 | 85 | 64-66 | 1.00 | 6—8 | 200 mesh pass rate 90-95% | White |
QM-80 | 80 | 60-64 | 1.00 | 8—10 | 200 mesh pass rate 90-95% | White |
QM-70-75 | 70-75 | 50-55 | 1.00 | 10-15 | 200 mesh pass rate 90-95% | special white |
Table of influence of storage time on magnesium oxide content (take 85% magnesium oxide as an example) (air humidity below 50%)
Storage age (days) | 15 | 25 | 40 | 60 | 80 |
Active MgO% content | 65 | 63 | 60 | 55 | 40 |
Active MgO/MgO amount | 0.79 | 0.75 | 0.69 | 0.55 | 0.40 |